All articles

Problems & fixes

How to Prevent Dimples in Epoxy Resin

A smooth, glossy finish is one of the most attractive features of epoxy resin art. However, small depressions or uneven spots can sometimes appear on the surface during curing, affecting the final appearance of your artwork. These imperfections are commonly called dimples. They may develop for several reasons, including temperature changes, surface contamination, excessive heat, or uneven resin coverage. Understanding what causes them is the first step toward preventing them.

What Causes Dimples in Epoxy Resin?

1. Temperature Fluctuations

Temperature changes during curing can affect how resin flows, levels, and hardens. When the surrounding temperature drops, resin becomes more viscous and may lose its ability to level evenly. Temperature changes can also contribute to uneven curing or surface irregularities, particularly when combined with other factors.

How to prevent it

  • Maintain a stable room temperature throughout the curing process, especially during the initial stages.

  • Follow the manufacturer’s recommended working and curing temperatures. Many art epoxies perform well around 22–25°C, although requirements vary.

  • Avoid placing your artwork near air-conditioning vents, heaters, or open windows.

  • Ensure the resin, hardener, mould, and work surface have reached a suitable temperature before pouring.

Tip: If you use air conditioning to regulate your workspace, stabilise the room temperature before pouring and avoid directing airflow toward the artwork. Sudden changes in temperature can interfere with consistent curing.

2. Dust and Airborne Particles

Dust, fibres, hair, and other airborne particles can settle on wet resin and disrupt its smooth surface. Depending on their size and composition, these contaminants may become embedded in the coating or create small surface depressions.

How to prevent it

  • Clean the workspace before preparing your resin.

  • Remove dust and loose particles from the artwork, mould, and surrounding surfaces.

  • Avoid sweeping, dusting, or creating unnecessary air movement immediately before pouring.

  • Cover the artwork with a clean, raised dust cover as soon as the pouring and bubble-removal process is complete.

Tip: Prepare your dust cover before mixing resin so you can protect the artwork immediately after pouring. Make sure the cover does not touch the wet surface.

3. Excessive Heat During Bubble Removal

A torch or heat gun can help release trapped air bubbles, but excessive heat may damage the resin surface.

Holding a heat source too close or concentrating it in one area can cause localised overheating, rapid bubbling, or surface irregularities.

How to prevent it

  • Use only the amount of heat necessary to release surface bubbles.

  • Keep the heat source moving rather than concentrating it on one spot.

  • Avoid repeatedly heating the same area.

  • Follow the resin manufacturer’s recommendations for bubble removal.

Important: Not all epoxy resins are suitable for torching. Open flames also present fire risks, particularly around flammable materials or vapours. Use a heat source only when the product manufacturer permits it.

4. Surface Contamination

One of the most common causes of small circular depressions is contamination on the surface beneath the resin.

Oil, silicone, wax, fingerprints, polishing products, and cleaning residues can interfere with the resin’s ability to spread evenly.

When resin pulls away from a contaminated area, it may leave a circular depression known as a fisheye, which can resemble a dimple.

How to prevent it

  • Make sure the surface is clean, dry, and free from grease or other residues.

  • Avoid touching the prepared surface with bare hands.

  • Remove sanding dust thoroughly before applying a new resin layer.

  • Use cleaning products compatible with both the substrate and the resin, following the manufacturer’s instructions.

Tip: Silicone contamination can be particularly difficult to remove. Keep silicone sprays, lubricants, and polishing products away from your resin workspace.

5. Insufficient Resin Coverage

An excessively thin coating may fail to level evenly, especially on textured or porous surfaces. As resin spreads, certain areas may become too thin, exposing the underlying texture or creating shallow depressions.

How to prevent it

  • Apply the resin within the manufacturer’s recommended coating thickness.

  • Calculate the required quantity before mixing.

  • Spread the resin evenly without excessively scraping or stretching it across the surface.

  • Seal porous materials when necessary to reduce absorption and air release.

Tip: Adding more resin is not always the solution. If the underlying surface is contaminated, the resin may continue to pull away even when a thicker layer is applied.

How to Fix Dimples in Cured Resin

If dimples have already appeared, the appropriate repair depends on their depth, extent, and underlying cause.

Step 1: Allow the Resin to Cure Completely

Do not begin sanding or recoating until the resin has reached the manufacturer’s specified cure stage for the intended repair.

Step 2: Inspect the Surface

Determine whether the imperfections are isolated depressions, widespread fisheyes, or pinholes caused by escaping air. Identifying the problem helps prevent it from recurring.

Step 3: Clean and Prepare the Surface

Remove any contamination using a suitable cleaning method. If necessary, sand the affected area or the entire surface to create a uniform finish and improve adhesion, following the manufacturer’s recoating instructions.

Step 4: Apply a Fresh Resin Layer

Once the surface is clean, dry, and properly prepared, apply a fresh, even coating of compatible epoxy resin. Maintain suitable curing conditions and protect the artwork from dust until the resin has hardened.

Important: Sanding alone will not remove silicone, oil, or other contaminants. The underlying cause must be addressed before recoating.

Final Thoughts

Preventing dimples in epoxy resin requires more than careful pouring. A clean surface, controlled temperature, appropriate coating thickness, and proper bubble-removal techniques all contribute to a smoother finish.

Although minor imperfections can often be repaired, identifying their cause before applying another coat is essential. With consistent preparation and suitable curing conditions, you can significantly reduce surface defects and achieve a more professional result.